Key points are not available for this paper at this time.
The corrosive zone at the anode of a proton exchange membrane water electrolyser extends only ∼200 μm into the porous transport layer under typical operating conditions, allowing replacement of platinum-coated titanium with much cheaper materials.
Becker et al. (Sat,) studied this question.