Los puntos clave no están disponibles para este artículo en este momento.
By adding l-arginine, cellulose degradation was inhibited in C4mimCl with a 90% regeneration rate after 24 h at 130 °C.
Yang et al. (Tue,) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: