Based on the present systematic review, all-ceramic crowns, when used for anterior teeth, showed survival rates at 5 years comparable to those seen for metal-ceramic crowns. When used for posterior teeth, the survival rates at 5 years of densely sintered alumina crowns (94.9%) and reinforced glass-ceramic crowns (93.7%) were similar to those obtained for metal-ceramic crowns. Furthermore, lower survival rates of 90.4% and 84.4% can be expected for InCeram crowns and glass-ceramic crowns when utilized for premolars and molars.