from 0.1 to 1.6 THz for this La:YIG film. Moreover, the THz Faraday rotation effect of La:YIG film was measured by the orthogonal polarization detection method in THz-TDS system, which can be actively manipulated by a weak longitudinal magnetic field of up to 0.155 T. With 5 samples stacked together, the Faraday rotation angle varies linearly from -15° to 15°, and the Verdet constant of La:YIG is about 100 °/mm/T within the saturation magnetization. This magneto-optical single crystal thick film with large area shows low loss, high permittivity and strong magneto-optical effect in the THz regime, which will be widely used in magneto-optical polarization conversion, nonreciprocal phase shifter and isolator for THz waves.