H-NMR, increased to 0.67 mmol/g for the HI-DL, and 0.64 mmol/g for the HBr-DL, from 0.52 mmol/g for the AL. These results showed that HI, a stronger nucleophilic reagent than HBr, provided a higher degree of AL demethylation. Lignin-containing resins, prepared by copolymerization, met the bonding strength standard for exterior plywood with DL used to replace as much as 50 wt.% of phenol. The increased hydroxyl contents resulting from the lignin demethylations also imparted faster cure times for the lignin-containing resins and lower formaldehyde emissions. Altogether, the stronger nucleophilicity of HI, compared to HBr, impacted the degree of lignin demethylation, and carried through to measurable differences the thermal properties and performance of the lignin-containing PF resins.