A significant difference exists in the marginal gap discrepancy when comparing hybrid ceramic and lithium disilicate CAD/CAM crowns. Also crystallization firing can result in a significant increase in the marginal gap of lithium disilicate CAD/CAM crowns.
Azarbal et al. (Thu,) studied this question.