and internal pressure changes during cycling were monitored as a sensitive indicator of gas evolution. Distinct categories of impurity behavior were identified, ranging from strongly HER-promoting noble metals to species whose apparent inertness arises from limited solubility. From these results, impurity-specific threshold ranges were established, defining the onset concentrations at which HER leads to irreversible pressure build-up. These thresholds provide practical guidance for setting vanadium liquid electrode purity specifications and highlight the inherent differences between sealed VIBs and conventional redox flow batteries. Collectively, this work bridges fundamental understanding of impurity-HER interactions with industrial requirements for liquid electrode management, enabling long-term stability and safe operation of sealed VIB systems.