Key points are not available for this paper at this time.
A process has been developed for the production of adherent nickel deposits of good quality on steel without the uSe of an electric current. The deposition of nickel is brought about by chemical reduction of a nickel salt with hypophosphites in a hot ammoniacal solution. The reaction is catalytic and, under the prescribed conditions of concentration and pH, no reduction occurs in the solution unless certain metals, such as steel or nickel, are introduced into the bath. The reduction then occurs only at the surface ot the immersed metal with the production of a coating of nickel of 96 to 97 percent purity.
Brenner et al. (Mon,) studied this question.