Statement of problemEvidence comparing the survival of zirconia crowns with metal-ceramic crowns is sparse. Knowledge of their survival and a comparison of their clinical outcomes would improve clinical decision making.PurposeThe purpose of this university-based study was to compare the survival, failures, biological and technical complications encountered with zirconia and metal-ceramic crowns restored and followed up over a similar period.Material and methodsThis retrospective chart review consisted of 403 patients treated at the University of Toronto, Faculty of Dentistry, predoctoral dental clinic in whom zirconia (n=209) and metal-ceramic (n=306) crowns were inserted between September 2015 and July 2016 and followed for up to 7 years. Outcome measures included failure, causes for failure, and complications associated with survival. Inferential statistical analysis included the chi-squared test, t test, Mann-Whitney test, Bonferroni-adjusted z-test, Kaplan-Meier survival test, and logistic regression to examine differences between crown types and explore crown failures (α=.05).ResultsThe mean follow-up period was 3.00 years (median 2.58 years). Forty-one (8.0%) crowns had no follow-up, with no difference in follow-up between crown type: metal-ceramic n=23(7.5%), zirconia n=18(8.6%), χ²(1)=0.20, P=.652). Excluding those with no follow-up, the follow-up time between metal-ceramic (mean=3.07, median=2.58) and zirconia (mean=3.54, median=3.32) crowns was statistically similar (P=.052). There were 62 anterior crowns (12.0%) and 453 posterior crowns (88.0%), χ²(1)=22.40, P<.001, with no difference between groups. Overall, 44 crowns (8.5%) failed, 30 (9.8%) metal-ceramic and 14 (6.7%) zirconia, with no statistical difference in proportion of failed crowns between groups (χ²(1)=1.53, P=.216). There were 35 crowns with biological failures (6.8%), 26 (8.5%) in the metal-ceramic and 9 (4.4%) in the zirconia group, with no statistical difference between groups (χ²(1)=3.33, P=.068). Nine crowns had technical failures (1.7%), 4 (1.4%) in the metal-ceramic group and 5 (2.5%) in the zirconia group, with no statistical difference between groups (χ²(1)=0.73, P=.394). Biological (79.5%) rather than technical complications were found to be the most frequent cause of failure, goodness-of-fit χ²(1)=15.36, P<.001. Tooth fracture (50.0%) specifically was found to be the most frequent cause of failure, χ²(3)=21.27, P<.001. The total number of crowns that survived was 471 (91.5%); 276 (90.1%) were metal-ceramic and 195(93.3%) zirconia. The survival time (years) for metal-ceramic was mean=6.26, 95% CI 6.01–6.51 and for zirconia crowns mean=6.54, 95% CI 6.31–6.77. Of the crowns that survived, 370 (78.6%) had no clinical complications, and 101 (21.4%) crowns demonstrated similar clinical complications, with no statistical differences between groups.ConclusionsWithin the study follow-up time, the survival of monolithic zirconia and metal-ceramic crowns was 91.5%, with similar clinical complications between groups. Biological complications, especially tooth fracture, were a significantly more frequent complication with both types of crowns.
Building similarity graph...
Analyzing shared references across papers
Loading...
Neena L. D’Souza
Emma ML Jutlah
Rachel A. Deshpande
Journal of Prosthetic Dentistry
University of Toronto
University of Waterloo
Sunnybrook Health Science Centre
Building similarity graph...
Analyzing shared references across papers
Loading...
D’Souza et al. (Mon,) studied this question.
synapsesocial.com/papers/68e70da3b6db6435876875a6 — DOI: https://doi.org/10.1016/j.prosdent.2024.02.028