Carbamide and Hydrogen Peroxide Bleaching Effect on Modern CAD/CAM Dental Ceramics: An Investigation on Ion Release and Surface Characteristics

View Full Paper
LVL VavrickovaJSJ. SchmidtMKM Kapitan

Key Points

  • To examine how carbamide and hydrogen peroxide bleaching agents affect dental ceramics.
  • Investigated CAD/CAM ceramics using SEM and ICP-OES analysis.
  • Applied varying concentrations of carbamide peroxide (10%, 20%, 30%) and hydrogen peroxide (35%, 40%) on ceramics.
  • Analyzed surface characteristics and elemental release post-treatment.
  • Ion release was significantly higher in feldspathic ceramics compared to other materials.
  • Surface changes occurred in all ceramics except lithium disilicate and zirconia-reinforced lithium silicate.
  • Bleaching agents did not significantly impact elemental composition or total mass loss.

Abstract

Objectives: This study aimed to investigate the impact of bleaching agents based on carbamide or hydrogen peroxide on dental ceramics in vitro, utilizing scanning electron microscopy (SEM) and elemental analysis via inductively coupled plasma optical emission spectroscopy (ICP-OES). Methods: CAD/CAM ceramics (IPS e.max®CAD, IPS Empress®CAD, Vitablocs® Mark II, Celtra Duo, and inCoris TZI) were treated with bleaching agents using either 10%, 20%, 30% carbamide peroxide or with 35%, and 40% hydrogen peroxide. Results: Surface elemental release was not significantly affected by the type or concentration of bleaching agent (p>0.05). Ion release in feldspathic ceramics was significantly higher than in other ceramic materials (p⟨0.0001). Microstructural surface changes were observed in all materials except for lithium disilicate and zirconia-reinforced lithium silicate ceramics. Conclusions: All bleaching agents tested in this study showed a similar impact within each material type tested regarding total mass loss, elemental composition, or surface structure. Clinical relevance: Lithium disilicate and zirconia-reinforced lithium silicate ceramics were the most resistant to bleaching agents. In contrast, feldspathic ceramic showed the highest ion release and surface deterioration when exposed to all bleaching agents tested.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Vavrickova et al. (2025) studied this question.

synapsesocial.com/papers/699a9dae482488d673cd3be5https://doi.org/10.5167/uzh-292233
Ask AI
Helpful
Bookmark
Share
View Full Paper