PulseExploreJournal ClubDebatesTrendingResearchersJournals
Instagram
HomeExploreJournal ClubTrending
Synapse
⌘+K
Synapse
March 29, 2026SHILAP Revista de lepidopterología0 citationsOpen Access

Comparative Study of Cork Tree Bark and Silanized Cork Tree Bark as Eco-Friendly Fillers for Various Elastomers – Ecological Approach to Green Rubber Composites

View Full Paper
KMKonrad MrozowskiASAleksandra Smejda-Krzewicka

Key Points

  • The aim is to assess the impact of silanized versus native cork tree bark as fillers in elastomeric composites and evaluate their performance.
  • The filler was modified using n-octadecyltrimethoxysilane.
  • Characterization methods included FTIR spectroscopy, contact angle measurements, and dynamic light scattering.
  • Rheometric characteristics and crosslink density were analyzed alongside mechanical properties.
  • Silanization increased hydrophobicity, with contact angles rising from 44.5° to 121.1°.
  • Mechanical strength of biocomposites improved, achieving 19.42 MPa tensile strength.
  • Wettability decreased notably in XNBR-based composites, contact angles increased from 33.6° to 98.5°.
  • Barrier properties showed reduced liquid and gas permeability across all composite systems.

Abstract

This study examines elastomeric composites reinforced with native and chemically modified lignocellulosic material derived from Amur cork tree bark, focusing on the effectiveness of filler modification and its impact on composite performance. The filler was modified using n-octadecyltrimethoxysilane, and the modification was evaluated by FTIR spectroscopy, contact angle measurements, and dynamic light scattering. Successful silanization was confirmed by characteristic FTIR signals, a marked increase in hydrophobicity (water contact angle from 44.5° to 121.1°), a reduction in surface free energy to 29.03 mN/m. The influence of silanization of filler on the properties of the filled composites was evaluated based on rheometric characteristics and crosslink density, mechanical properties, surface, and barrier properties. A notable improvement in the mechanical strength of the biocomposites was observed (TSb = 19.42 MPa). A significant reduction in wettability was also recorded, particularly for XNBR-based composites, where the water contact angle increased from 33.6° to 98.5°. Furthermore, enhanced barrier properties were achieved, as evidenced by reduced liquid and gas permeability for all filled composite systems (1.6–7.3 × 10−13 mol/(Pa·m·s)). Overall, the results demonstrate proper functional properties while maintaining environmental benefits and highlight promising directions for the development of elastomeric biomaterials.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Mrozowski et al. (2026) studied this question.

synapsesocial.com/papers/69c8c0b0de0f0f753b39b96chttps://doi.org/10.1080/15440478.2026.2646162
Ask AI
Helpful
Bookmark
Share
View Full Paper

Also Consider

Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context:

  1. 1Effect of Modified and Unmodified Oak Bark (Quercus Cortex) on the Cross-Linking Process and Mechanical, Anti-Aging, and Hydrophobic Properties of Biocomposites Produced from Natural Rubber (NR)2024 · 13 citations
  2. 2Green biocomposites of chitosan dispersed in natural rubber matrices, and their urea controlled-release application2020 · 13 citations
  3. 3Wettability Study on Natural Rubber Surfaces for Applications as Biomembranes2018 · 23 citations