July 21, 2017Advanced Energy Materials685 citationsOpen Access

“Water‐in‐Salt” Electrolyte Makes Aqueous Sodium‐Ion Battery Safe, Green, and Long‐Lasting

View Full Paper
LSLiumin SuoOBOleg BorodinYWYuesheng Wang

Key Points

Key points are not available for this paper at this time.

Abstract

Abstract Narrow electrochemical stability window (1.23 V) of aqueous electrolytes is always considered the key obstacle preventing aqueous sodium‐ion chemistry of practical energy density and cycle life. The sodium‐ion water‐in‐salt electrolyte (NaWiSE) eliminates this barrier by offering a 2.5 V window through suppressing hydrogen evolution on anode with the formation of a Na + ‐conducting solid‐electrolyte interphase (SEI) and reducing the overall electrochemical activity of water on cathode. A full aqueous Na‐ion battery constructed on Na 0.66 Mn 0.66 Ti 0.34 O 2 as cathode and NaTi 2 (PO 4 ) 3 as anode exhibits superior performance at both low and high rates, as exemplified by extraordinarily high Coulombic efficiency (>99.2%) at a low rate (0.2 C) for >350 cycles, and excellent cycling stability with negligible capacity losses (0.006% per cycle) at a high rate (1 C) for >1200 cycles. Molecular modeling reveals some key differences between Li‐ion and Na‐ion WiSE, and identifies a more pronounced ion aggregation with frequent contacts between the sodium cation and fluorine of anion in the latter as one main factor responsible for the formation of a dense SEI at lower salt concentration than its Li cousin.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Suo et al. (2017) studied this question.

synapsesocial.com/papers/69d750b3b1cb92dd1bb8a6cbhttps://doi.org/10.1002/aenm.201701189
Ask AI
Helpful
Bookmark
Share
View Full Paper