January 1, 2009Journal of The Electrochemical Society265 citations

Cycle-Life Characterization of Automotive Lithium-Ion Batteries with LiNiOsub 2 Cathode

View Full Paper
YZYancheng ZhangCWChao‐Yang Wang

Key Points

Key points are not available for this paper at this time.

Abstract

A set of lithium-ion cells containing a -based positive electrode and a graphite negative electrode were cycled nonintrusively at high power (5C rate) and elevated temperature . The aged cells were characterized at prescribed cycle numbers (up to 5250 cycles) by a three-electrode cell, capacity measurement, and electrochemical impedance spectroscopy (EIS). Excellent cyclability of these cells under typical hybrid-electric vehicle conditions is demonstrated by 18% capacity fade after 5250 cycles, and the discharge capacity shows a mainly parabolic behavior with the cycle number (dependent on ) in the initial stage and a linear behavior (dependent on ) for subsequent cycles. Using a lithium reference electrode further reveals that the capacity fade during cycling is primarily caused by the positive electrode, where discharge capacity may be limited by a decrease in active lithium intercalation sites in the oxide particles. The increase in full-cell impedance with cycling is evident from the increase in midfrequency arc width , composed of charge-transfer kinetic resistance and transport resistance through the solid electrolyte interphase (SEI), . More specifically, the cell-impedance rise comes mainly from the rising and of the positive electrode. Based on individual electrode EIS spectra and equivalent-circuit analysis, it is found that the rise in the positive electrode is far more influential than the change in . Therefore, property modification and thickening of the SEI layer of the positive electrode during cycling appear to be dominant factors in cell-impedance rise and power fade.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Zhang et al. (2009) studied this question.

synapsesocial.com/papers/69daccf3ed2e131d3c68445ehttps://doi.org/10.1149/1.3126385
Ask AI
Helpful
Bookmark
Share
View Full Paper

Also Consider

Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context:

  1. 1Design considerations2021 · 139 citations
  2. 2Electrochemical and Thermal Behavior of LiNi1 − z M z O 2 ( M = Co , Mn , Ti )1997 · 194 citations
  3. 3Development of Reliable Three-Electrode Impedance Measurements in Plastic Li-Ion Batteries2001 · 160 citations
  4. 4Comparison of the chemical stability of the high energy density cathodes of lithium-ion batteries2001 · 183 citations
  5. 5Stabilization of the layered crystal structure of LiNiO2 by Co-substitution1993 · 238 citations