May 26, 2026Metals1 citationsOpen Access

Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and Fracture

View Full Paper
BYBoris YanachkovKVKateryna ValuiskaYMYana Mourdjeva

Key Points

  • The aim is to elucidate the mechanisms of hydrogen embrittlement in welded joints of pipeline steel from a gas network.
  • Investigated welded joints in X52 pipeline steel after 31 years of service.
  • Used X-ray diffraction, electrochemical hydrogen permeation, and transmission electron microscopy analyses.
  • Conducted fractographic analysis to assess changes in fracture behavior under hydrogen exposure.
  • Production weld shows significantly lower diffusion coefficient and five times greater hydrogen trap density than girth weld.
  • Ductile to brittle fracture transition observed, with 53% brittle zones in hydrogen-charged specimens.
  • Outer-wall specimens exhibit greater hydrogen susceptibility due to combined long-term corrosion and degradation.

Abstract

This study investigates hydrogen embrittlement in welded joints of X52 (L360) pipeline steel obtained from an operating natural gas transmission network after 31 years of service, with particular emphasis on production (longitudinal) and girth (circumferential) welds. The aim is to elucidate the influence of microstructural heterogeneity across the pipe wall and within different welded joint types on hydrogen transport, trapping behavior, and fracture mechanisms. The investigation combines X-ray diffraction, electrochemical hydrogen permeation testing, fractographic analysis, and transmission electron microscopy. X-ray diffraction results show that the base metal and girth weld consist predominantly of body-centered cubic ferrite, whereas the production weld additionally contains retained austenite associated with an elevated manganese content. These phase-related differences are consistent with transmission electron microscopy observations of martensite–austenite constituents within the weld microstructure. Electrochemical hydrogen permeation measurements reveal pronounced microstructure-dependent hydrogen transport behavior. The production weld exhibits a significantly lower apparent diffusion coefficient and a markedly higher hydrogen trap density, approximately five times greater than those of the base metal and girth weld, providing a mechanistic explanation for the observed differences in hydrogen uptake behavior. Fractographic analysis demonstrates a transition from ductile microvoid coalescence in the uncharged condition to predominantly brittle fracture following hydrogen charging. This transition is accompanied by a substantial increase in the fraction of brittle fracture zones, reaching approximately 53% in hydrogen-charged specimens. A pronounced gradient in hydrogen embrittlement susceptibility is observed across the pipe wall thickness, with outer-wall specimens consistently exhibiting greater susceptibility than inner-wall specimens. This behavior reflects the combined influence of long-term soil corrosion and hydrogen-assisted degradation. Transmission electron microscopy reveals that plastic deformation governs dislocation generation, while hydrogen significantly modifies dislocation behavior by promoting dislocation pile-ups near martensite–austenite constituents and non-metallic inclusions. These observations indicate strong interactions between hydrogen, dislocations, and microstructural heterogeneities. A clear size-dependent role of non-metallic inclusions is identified. Sub-micron inclusions act primarily as irreversible hydrogen trapping sites that contribute to hydrogen redistribution within the microstructure, whereas larger inclusions serve as preferential crack initiation sites under hydrogen charging conditions. Overall, the results demonstrate that hydrogen embrittlement behavior is governed by the combined effects of microstructural state, welded joint type, and long-term service-induced degradation, resulting in distinct hydrogen transport characteristics and fracture responses across the pipe wall.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Yanachkov et al. (2026) studied this question.

synapsesocial.com/papers/6a153a88b5d9c58d83e8d254https://doi.org/10.3390/met16060573
Ask AI
Helpful
Bookmark
Share
View Full Paper