July 15, 1969Physical Review24 citations

Electrical Studies of Electron-Irradiated Lithium-Containingn-Type Silicon

View Full Paper
GBG. J. Brucker

Key Points

Key points are not available for this paper at this time.

Abstract

Hall-coefficient and resistivity measurements have been used to investigate the crystal growth and irradiation-temperature dependence of the introduction rate and room-temperature annealing of carrier-removal defects in lithium-doped silicon. Initial resistivity of the quartz-crucible silicon was 30 cm and of the float-zone silicon was 1500 cm. The silicon was doped with lithium to a density of 210^16 cm^-3. Irradiations were carried out with 1-MeV electrons at bombardment temperatures ranging from 79 to 280^. Specimens were annealed to 200^, thereby separating intrinsic and impurity defects. Introduction rates of carrier-removal defects were exponentially dependent on the reciprocal of temperature for both types of crystal, but the slopes and limiting temperature values differed. The slope of the carrier-removal rate versus reciprocal temperature curve is 0. 055 eV in crucible silicon and 0. 09 eV in zone-refined silicon. The temperature dependence was not consistent with a simple charge-state-dependent probability of interstitial-vacancy dissociation and impurity-vacancy trapping. Carrier concentrations measured at or near room temperature were increased in zone silicon, but were decreased in crucible silicon by isothermal annealing at room temperature. Crucible-silicon samples annealed to 373^ for 10 min exhibited complete recovery of mobility. Complete recovery of mobility in float-zone-refined silicon took place in an annealing time 17 h at room temperature. The time constant of the annealing kinetics at room temperature is consistent with the observation that the lithium-diffusion constant in oxygen-rich silicon is smaller than that in oxygen-lean silicon. The mechanism of room-temperature annealing is attributed to neutralization of carrier-removal defects by lithium interaction in crucible silicon, and by both lithium interaction and defect dissociation in zone-refined silicon. Results suggest that radiation produces a lithium-oxygen-vacancy complex in quartz-crucible-grown silicon, and a lithium-vacancy complex in float-zone-refined silicon. The LiO-V defect is tightly bound compared to the oxygen-free Li-V defect. Measurements of carrier density as a function of reciprocal temperature located defect-energy levels near E₂- (0. 18 eV) and E₂- (0. 13 eV), in irradiated-crucible silicon. The former defect level is the A center, and the latter is the reverse annealing center, which is formed at a temperature of 250^. A defect level located near E₂- (0. 08 eV) formed after crucible-silicon samples were annealed at room temperature and lithium interacted with radiation defects.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

G. J. Brucker (1969) studied this question.

synapsesocial.com/papers/6a6f2cbe2163a0a01bc381e0https://doi.org/10.1103/physrev.183.712
Ask AI
Helpful
Bookmark
Share
View Full Paper