Fe3O4 Nanoparticles Functionalized with Polymer Ligand for T1-Weighted MRI In Vitro and In Vivo

CXChenyang XiangXZXin ZhongWYWeitao Yang

Key Points

Key points are not available for this paper at this time.

Abstract

Magnetic resonance imaging (MRI) has gained wide interest in early accurate diagnoses due to the high resolution and low toxicity of magnetic nanoparticles. In order to develop potential alternatives of toxic Gd- or Mn-based chelating agents, we report the synthesis of water soluble ultra-small Fe3O4 nanoparticles by a modified co-precipitation method as T1-weighted positive contrast agents. The magnetic iron oxide nanoparticles (MIONs) were functionalized by polymer ligand dodecanthiol-polymethacrylic acid (DDT-PMAA) to enhance their colloidal stability. These MIONs have high longitudinal relaxivity (r1 = 8.18 mM−1·S−1) and exhibited good results in the in vitro and in vivo MR imaging. No toxicity was observed in cytotoxicity assay and histology toxicity analysis. The MIONs@DDT-PMAA(magnetic iron oxide nanoparticles @ dodecanthiol-polymethacrylic acid) present great potential as positive contrast agents for tumor diagnosis.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Xiang et al. (2019) studied this question.

synapsesocial.com/papers/6a89b6884c30e1095aec8909https://doi.org/10.3390/polym11050882
Ask AI
Helpful
Bookmark
Share
View Full Paper