September 3, 2005Chemistry of Materials29 citations

Crystallization of Highly Oriented ZnO Microrods on Carboxylic Acid-Terminated SAMs

View Full Paper
RTR. TurgemanOGOlga GershevitzMDMoshe Deutsch

Key Points

Key points are not available for this paper at this time.

Abstract

Highly oriented microrods ZnO crystals having a narrow size distribution were successfully crystallized on Si wafers coated with SiCl 3 (CH 2 ) 11 −O−C 6 H 4 −COOH. The relationship between surface properties and the crystallization products was investigated by ellipsometry, wetting measurements, X-ray reflectivity (XR), and grazing incidence diffraction (GID). The influence of the phenyl ether chromophore and the carboxylic group were explored by comparing the crystallization products obtained on monolayers made from SiCl 3 (CH 2 ) 11 −O−C 6 H 4 −COOCH 3, SiCl 3 (CH 2 ) 16 −COOH, and SiCl 3 (CH 2 ) 16 −COOCH 3 molecules. The results demonstrate that the carboxylic acid end group is crucial for achieving a highly oriented growth.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Turgeman et al. (2005) studied this question.

synapsesocial.com/papers/6a90fe9f073a0b1e9f744e5chttps://doi.org/10.1021/cm051234q
Ask AI
Helpful
Bookmark
Share
View Full Paper