This article shows improved performance in zinc anodes and cathodes using bifunctional additives, suggesting vital applications.
Aqueous zinc-ion batteries have garnered significant attention due to their high safety, cost-effectiveness, and environmental sustainability. However, the performance of the zinc anode is considerably compromised by hydrogen evolution, corrosion, and structural degradation of the cathode. This article provides a detailed discussion of a mixture comprising ZnSO4, Zn(OTf)2, and NH4Cl as electrolytes in zinc-ion batteries. The incorporation of additives such as Zn(OTf)2 and NH4Cl not only facilitates the effective formation of a solid-electrolyte interphase containing ZnF2 and Zn3N2 but also mitigates the hydrolysis of the cathode material NH4V4O10. Symmetric batteries assembled with bifunctional additives as anodes can achieve a low current density of 1 mA cm-2 for over 900 h and sustain a higher current density of 5 mA cm-2 for more than 570 h. Furthermore, the NH4V4O10//Zn full battery utilizing bifunctional additives maintains a Coulombic efficiency rate of up to 99.99% after 2000 cycles at a current density of 1 A g-1. This bifunctional additive is anticipated to play an increasingly pivotal role in practical applications and advanced aqueous-based zinc-ion battery technology.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2025) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: