Designing Effective Electronic Barriers at Grain Boundaries in Garnet for Improved Cycling Performance in Solid-State Lithium Batteries

View Full Paper
XXXing XiangChongqing UniversityZZZhenzhen ZhaoShenyang Pharmaceutical UniversityJCJiajia ChenChongqing University of Posts and Telecommunications

Key Points

  • Enhanced capacity retention of 89.7% after 200 cycles at room temperature improves overall battery longevity.
  • Critical current density increased from 0.4 to 0.8 mA·cm–2, ensuring better cycling performance during operation.
  • Modification of grain boundaries using LiCl effectively restricts electron migration, combatting lithium dendrite formation.
  • Operation stability exceeded 2000 hours at 0.3 mA·cm–2, showcasing the robustness of the modified batteries.

Abstract

Solid-state lithium batteries (SSLBs) have emerged as a promising successor to conventional lithium batteries owing to their outstanding safety and elevated energy storage capabilities. Among various solid electrolytes used in SSLBs, Li7La3Zr2O12 (LLZO) is renowned for its superior performance. However, its high electronic conductivity, especially at grain boundaries, promotes lithium dendrite formation, compromising battery performance. To address this issue, we engineered continuous grain boundaries with electron–blocking properties in LLZO to inhibit lithium dendrite growth. Due to the limited incorporation of Cl into the LLZO lattice, excess LiCl accumulates at grain boundaries, effectively restricting electron migration. This approach avoids excessive doping of secondary-phase elements into the LLZO lattice, which could degrade the grain properties. After modification, symmetric lithium batteries with LiCl–LLZO exhibit an increased critical current density from 0.4 to 0.8 mA·cm–2 (time-constant mode) and operate stably for over 2000 h at 0.3 mA·cm–2. The batteries using LiFePO4 as the cathode achieve 89.7% capacity retention (133.5 mAh·g–1) after 200 cycles at room temperature and 0.2 C. These findings confirm that this strategy successfully hinders lithium dendrite growth and enhances battery performance.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Xiang et al. (2025) studied this question.

synapsesocial.com/papers/68c1d7ee54b1d3bfb60f9dc6https://doi.org/10.1021/acssuschemeng.5c04208