In this study, crack-free TiC/Ti composites with TiC content ranging from 0 to 15 wt.% were successfully fabricated using Direct Energy Deposition with a dual-feeder system that concomitantly delivered different amounts of both constituents into a high-power laser beam. The samples were investigated to evaluate the morphologies and distribution behavior of TiC. The microhardness values of the samples obtained under optimal processing conditions increased from 192 ± 5.3 HV