This study is to propose time-variant probabilistic models of surface chloride and diffusion coefficient based on the survey data of 16 concrete bridge decks with the attack of de-icing salts. These models are developed, because there is no study that simultaneously considers both time-variance and probabilistic descriptors in the model for concrete bridge decks. From the study, it can be found that long-term surface chloride and its time-variant development are fitted with Log-normal and Weibull distributions, respectively. In addition, the 28-day diffusion coefficient and age factor are fitted with Log-logistic and Triangular distributions, respectively. Considering only the mean value in the models, the corrosion-free residual life of concrete bridge decks is equal to 18.3 years based on the target value of critical chloride of 1.2 kg/m 3 , whereas their cracking-free residual life is equal to 29.5 years based on the target value of critical chloride of 2.0 kg/m3. In comparison with the probabilistic analysis, it was nevertheless found that at year 18.3, there are 38% and 20% probabilities to have rebar corrosion and concrete cracking, respectively. However, at year 29.5, there are 63% and 42% probabilities to have rebar corrosion and concrete. Specifically, there are 6 and almost 7 out of 16 bridge locations having rebar corrosion in the year 18.3 and concrete cracking in the year 29.5, respectively.
No takes yet. Share an insight, caveat, or question.
Aruz et al. (2024) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: