October 8, 2025Polymers3 citationsOpen Access

Influence of Post-Washing Time and Build Orientation on Mechanical Properties and Biocompatibility of Additively Manufactured Permanent Dental Resin Material

View Full Paper
PPPei‐Wen PengJCJia-Syuan ChouLCLe-Xin Chen

Key Points

  • Post-washing for 90 seconds maximized water absorption, enhancing dental resin quality related to biocompatibility.
  • Flexural strength was highest at 0° build orientation, indicating how orientation affects the structural integrity of dental materials.
  • Post-washing time positively influenced cell viability, peaking at 150 seconds, which may improve patient outcomes in dental applications.
  • Build orientation impacted dimensional accuracy, with the least deviation seen in thickness, underscoring the importance of manufacturing parameters.

Abstract

Background: Digital light processing (DLP) is widely used in permanent dental restorations for its precision and efficiency, yet the effects of build orientation and post-washing time on resin properties remain unclear. This study aims to investigate the factors that impact the performance and biocompatibility of DLP-printed dental resins. Methods: Specimens were additively manufactured using permanent dental resin at 0°, 15°, and 90° orientations and post-washed for 90, 120, or 150 s. Evaluated properties included dimensional accuracy, hardness, flexural strength and modulus, degree of conversion, water sorption/solubility, and cytotoxicity. Results: Build orientation and post-washing time significantly affected dimensional accuracy, with thickness showing the least deviation. Flexural strength (p < 0.001) and modulus (p < 0.01) were highest at the 0° orientation. Post-washing for 90 s led to the greatest water absorption, while solubility remained unaffected. Cell viability increased with longer post-washing times, peaking at 150 s, with significant effects observed on days 5 and 7 (p < 0.05). Conclusions: Build orientation significantly affected dimensional accuracy and flexural strength, while post-washing time had minimal impact on physical properties. Notably, extended post-washing improved cell viability and reduced cytotoxicity, indicating its potential to enhance the clinical biocompatibility of DLP-fabricated dental resin.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Peng et al. (2025) studied this question.

synapsesocial.com/papers/68e5c1b46950a706b22b503chttps://doi.org/10.3390/polym17192694
Ask AI
Helpful
Bookmark
Share
View Full Paper