Commercial nickel foam (NF), which is composed of numerous interconnected ligaments and hundred-micron pores, is widely acknowledged as a current collector/electrode material for catalysis, sensing, and energy storage applications. However, the commonly used NF often does not work satisfactorily due to its smooth surface and hollow structure of the ligaments. Herein, a gas-phase-induced engineering, two-step gaseous oxidation-reduction (GOR) is presented to directly transform the thin-walled hollow ligament of NF into a three-dimensional (3D) nanoporous prism structure, resulting in the fabrication of a unique hierarchical porous nickel foam (HPNF). This 3D nanoporous architecture is achieved by utilizing the spontaneous reconstruction of nickel atoms during volume expansion and contraction in the GOR process. The process avoids the involution of acid-base corrosion and sacrificial components, which are facile, environmentally friendly, and suitable for large-scale fabrication. Furthermore, MnO
No takes yet. Share an insight, caveat, or question.
Wang et al. (2024) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: