April 1, 2026Polymer Engineering and Science1 citations

Strength and Interlayer Toughness of FDM PC , ABS , and PETG : Roles of Printing Speed and Environmental Temperature

View Full Paper
MSMirsadegh SeyedzavvarCBCem Boğa

Key Points

  • The aim is to evaluate the strength and toughness of FDM 3D printed PC, ABS, and PETG by varying printing speed and environmental temperature.
  • Conducted tensile and delamination tests at various temperatures (25/60/100°C) and printing speeds (50-150 mm/s).
  • Used Differential Scanning Calorimetry (DSC) and Fourier Transform Infrared Spectroscopy (FTIR) to analyze thermal transitions and chemical properties.
  • Developed a minimal model to describe interlayer healing and tensile retention based on temperature and speed.
  • PC showed the highest tensile strength across all temperatures but lower interlayer toughness compared to ABS and PETG.
  • PETG had the best delamination toughness at moderate temperatures but lost strength near 100°C.
  • ABS maintained stability up to 60°C but dropped in performance significantly at 100°C due to softening.

Abstract

ABSTRACT This work compares Polycarbonate (PC), Acrylonitrile–Butadiene–Styrene (ABS), and polyethylene terephthalate glycol (PETG) printed by fused deposition modeling (FDM) across speeds (50–150 mm/s) and test temperatures for mechanical characterization (tensile and delamination at 25/60/100°C), and interprets the results with a compact physics‐guided framework. Tensile and compact‐tension (CT) delamination tests, paired with Differential Scanning Calorimetry (DSC) and Fourier Transform Infrared Spectroscopy (FTIR), link thermal transitions and chemistry to performance. PC consistently delivers the highest bulk tensile strength at all temperatures/speeds (high glass transition temperature ( T g ), strong thermal stability) but shows lower interlayer resistance than ABS and PETG at 25°C–60°C unless printing is tuned. PETG provides the strongest delamination toughness at 25°C–60°C, especially at higher speeds, yet loses load‐bearing capacity near 100°C as it softens above T g . ABS is intermediate, remaining stable to 60°C and dropping sharply at 100°C primarily from matrix softening, consistent with DSC/FTIR. A minimal model, composed of (i) a reptation‐controlled interlayer‐healing term driven by nozzle temperature and residence time (speed), (ii) a monotone tensile‐retention law versus reduced temperature ( T env – T g ), and (iii) cohesive‐zone parameters inferred from CT, captures these trends and yields material‐specific speed–temperature maps. Practically, PC suits hot‐service (~100°C) if interlayer bonding is enhanced; PETG is optimal at room‐to‐moderate temperatures when delamination resistance is critical; ABS offers a balanced option when service temperatures stay well below T g .

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Seyedzavvar et al. (2026) studied this question.

synapsesocial.com/papers/69cd7b475652765b073a92c2https://doi.org/10.1002/pen.70441
Ask AI
Helpful
Bookmark
Share
View Full Paper

Also Consider

Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context:

  1. 1Effect of process parameters on the mechanical performance of FDM printed carbon fiber reinforced PETG2024 · 70 citations
  2. 2Thermomechanical and Viscoelastic Characterization of Continuous GF/PETG Tape for Extreme Environment Applications2024 · 5 citations
  3. 3Parametric analysis of additively manufactured polymer nanocomposites: A experimental and multiscale study2024 · 10 citations
  4. 4Fused filament fabrication of Nylon beyond the glass transition temperature in a thermally-insulated machine2023 · 5 citations
  5. 5Printing parameters and materials affecting mechanical properties of FDM-3D printed Parts: Perspective and prospects2021 · 251 citations