Increasing oxidation time during fabrication of hematite (Fe₂O₃) films reduces the amount of grain boundaries, resulting in lower flat band potential and onset potential for water oxidation.
No takes yet. Share an insight, caveat, or question.
Iandolo et al. (2015) studied this question.