We show that yttrium‐stabilized zirconia can be sintered in a few seconds at ∼850°C to full density, starting from a green density of 0.5, by the application of a dc electrical field (nominally, several hours at 1450°C are needed to complete the sintering process). This finding is explained by the local Joule heating at grain boundaries, which, on the one hand, promotes grain‐boundary diffusion (a kinetic effect), while at the same time restricts grain growth (a thermodynamic effect). The smaller grain size and the higher temperature at grain boundaries can then act synergistically to enhance the rate of sintering. These results have a bearing in explaining the widespread spark plasma and microwave‐assisted techniques for enhanced sintering.
Building similarity graph...
Analyzing shared references across papers
Loading...
Marco Cologna
Joint Research Centre
Boriana Rashkova
Austrian Academy of Sciences
Rishi Raj
Galgotias University
Journal of the American Ceramic Society
University of Colorado Boulder
Austrian Academy of Sciences
Erich Schmid Institute of Materials Science
Building similarity graph...
Analyzing shared references across papers
Loading...
Cologna et al. (Tue,) studied this question.
synapsesocial.com/papers/69d94efb9873513554835ebd — DOI: https://doi.org/10.1111/j.1551-2916.2010.04089.x
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: