After thermocycling, surface treatment had a significant effect on water contact angle and surface roughness. CLP or PK application resulted in hydrophobic surfaces compared with before thermocycling. CLP or SSC application on CAD-CAM PMMAs resulted in smoother surfaces. Thermocycling lowered the microhardness of all PMMAs, and the decrease was significant in CLP- or PK-applied PMMAs, except for PK-applied Poli.