Answers are grounded in this paper and cite their sources.
Both MMAs tested can be considered effective alternatives for bonding to sandblasted indirect resin composite after aging, as they showed similar bond performance to that of the control group. However, separate bottles of silane bonding resin showed higher MSBS values and more durable bonding for etched glass-based ceramic.
No takes yet. Share an insight, caveat, or question.
Makishi et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: