June 10, 2013Langmuir978 citations

Characterization of Polydopamine Thin Films Deposited at Short Times by Autoxidation of Dopamine

View Full Paper
RZRebecca A. ZangmeisterTMTim MorrisMTMichael J. Tarlov

Key Points

Key points are not available for this paper at this time.

Abstract

Current interest in melanin films derived from the autoxidation of dopamine stems from their use as a universal adhesion layer. Here we report chemical and physical characterization of polydopamine films deposited on gold surfaces from stirred basic solutions at times ranging from 2 to 60 min, with a focus on times ≤10 min. Data from Fourier transform infrared (FTIR), X-ray photoelectron spectroscopy (XPS), and electrochemical methods suggest the presence of starting (dopamine) and intermediate (C=N-containing tautomers of quinone and indole) species in the polydopamine films at all deposition times. A uniform overlayer analysis of the XPS data indicates that film thickness increased linearly at short deposition times of ≤10 min. At deposition times ≥10 min, the films appeared largely continuous with surface roughness ≈ ≤ 2 nm, as determined by atomic force microscopy (AFM). Pinhole-free films, as determined by anionic redox probe measurements, required deposition times of 60 min or greater.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Zangmeister et al. (2013) studied this question.

synapsesocial.com/papers/69dce63fd7a2ed3138133505https://doi.org/10.1021/la400587j
Ask AI
Helpful
Bookmark
Share
View Full Paper