The ring-opening polymerization of L-lactic acid O-carboxyanhydrides was initiated by triisopropoxyneodymium in toluene-THF mixtures. Typically, high yields and relatively high molecular weight PLAs were obtained within 4 h at 25 °C. The reaction was highly controllable and easy to conduct, and the molecular weight distribution of the PLAs was rather narrow (Mw/Mn = 1.10-1.36). NMR analysis showed that one end of the PLA chain consisted of an isopropoxy group, while the other end of the chain contained a hydroxyl group. Due to their availability and high polymerizability, Lac-OCAs are promising monomers for the preparation of tailored architectures derived from well-defined PLAs.