Key result
An ultrasonic atomization spray process successfully produced a PLLA coating incorporating GP IIIa mAb on stents, achieving a maximum mAb concentration of 1662 ng and 80% elution over 2 weeks in vitro.
Ultrasonic atomization is an effective method for creating a uniform PLLA coating for mAb-eluting stents with sustained release over 2 weeks in vitro.
Supports mAb-eluting stent development; leaves open in vivo efficacy and clinical translation.
An eluting-stent system with mAb dispersed in the PLLA (poly (L-lactic acid)) was validated in vitro. Specifically designed spray equipment based on the principle of ultrasonic atomization was used to produce a thin continuous PLLA (poly (L-lactic acid)) polymer coating incorporating monoclonal antibody (mAb). This PLLA coating was observed in light microscopy (LM) and scanning electron microscopy (SEM). The concentration of the monoclonal antibody (mAb) to the platelet glycoprotein (GP) IIIa receptor and the eluting rate were then measured by a radioisotope technique with (125)I-labelled GP IIIa mAb. An in vitro perfusion circuit was designed to evaluate the release rates at different velocities (10 or 20 ml min(-1)). The PLLA coating was thin and transparent, uniformly distributed on the surface of the stent. Three factors influenced its thickness: PLLA concentration, duration and gas pressure. The concentration of mAb was influenced by the duration of absorption and the concentration of the mAb solution; the maximum was 1662.23 + or - 38.83 ng. The eluting rate was fast for the first 2 h, then decreased slowly and attained 80% after 2 weeks. This ultrasonic atomization spray equipment and technological process to prepare protein eluting-stents were proved to be effective and reliable.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2009) studied this question. PLLA polymer coating incorporating monoclonal antibody (mAb) to GP IIIa receptor was evaluated on Eluting rate and coating characteristics. An ultrasonic atomization spray process successfully produced a PLLA coating incorporating GP IIIa mAb on stents, achieving a maximum mAb concentration of 1662 ng and 80% elution over 2 weeks in vitro.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: