In this work, the depressing effect of clay minerals on the floatability of chalcopyrite using PAX as collector was assessed through induction time and settling-turbidity measurements. The data obtained using these two techniques were correlated with the results of micro-flotation tests carried out to study the effect of kaolinite and smectite particles on the floatability of chalcopyrite at pH 9 and 10. The results indicate that these techniques can be confidently used to examine interactions between clay minerals and chalcopyrite, and their possible consequences on the flotation process. In particular, the use of settling-turbidity measurements to evaluate slime coating seems to be a useful technique that could be applied to study heterocoagulation in other mineral systems. It was found that the depressing effect of clay minerals was stronger at pH 10, which was correlated to a possible effect of Ca2+ from lime on the process of coagulation between clay minerals and chalcopyrite. Coating of bubbles with clays was detected in this work by visual observations and it is proposed as a mechanism that might explain the depressing effect of clays on the floatability of chalcopyrite. Further research is needed to propose a mechanism that explains this phenomenon.
No takes yet. Share an insight, caveat, or question.
Uribe et al. (2016) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: