The Pt/TiO 2, Pt/ZrO 2, and Pt/Al 2 O 3 catalysts submitted to low-temperature reduction (LTR, 200 °C) and high-temperature reduction (HTR, 500 °C) and exposed to hydrogen and carbon monoxide at room temperature were studied by infrared spectroscopy. There is a strong loss of transmission in the entire infrared spectra on Pt/TiO 2 after its exposure to hydrogen, which is related to the reducibility of the support. A typical SMSI behavior (strong metal−support interaction), such as the decrease in carbon monoxide adsorption capacity, was detected on Pt/TiO 2 and Pt/ZrO 2 after exposure to hydrogen, even for the catalysts submitted to LTR treatment. Also a carbonyl band shift to lower wavenumber was observed on LTR-treated Pt/TiO 2, Pt/ZrO 2, and Pt/Al 2 O 3 after exposure to hydrogen. We interpreted this SMSI behavior as an electronic rather than morphological effect, which was induced by the presence of hydrogen spillover.
No takes yet. Share an insight, caveat, or question.
Benvenutti et al. (1999) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: