The synthesis of three different poly(ethylene oxide) macromonomers with a norbornene and oxanorbornene end group is presented. The macromonomers were polymerized to comb‐polymers by ring‐opening metathesis polymerization (ROMP) using Grubbs' Catalyst G3 to produce water soluble polymers with polydispersities between 1.04 and 1.30 and molecular weights between 14,000 and 50,000 g/mol. Characterization by static and dynamic light scattering reveals that the comb‐polymers with norbornene backbone are molecularly disperse in aqueous solution, while the oxanorbornene‐backbone polymers form small water‐soluble aggregates.