The authors describe the results of a systematic study of the performance of silicone rubber terminations under contaminated conditions. The terminations evaluated were of the 15 kV class cold shrink type for concentric neutral cables. They were evaluated in a fog chamber where the electric stress, water conductivity, water flow rate, and the deenergization time between subsequent fog chamber exposures were varied in order to alter the test severity. Changes in the surface hydrophobicity were monitored periodically by analyzing the samples using ESCA (electron spectroscopy for chemical analysis), SEM (scanning electron microscopy), and contact angle measuring techniques. The results indicate that the experimental conditions play a significant role in the outcome of the tests. It was demonstrated that the recovery of hydrophobicity can be studied by using several techniques.>
No takes yet. Share an insight, caveat, or question.
Gorur et al. (1991) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: