Polystyrene (PS) microfibers with high molecular orientation and helical alignment were in situ formed via helical convergent flow during polybutene-1 (PB-1) tubing processing to achieve performance improvements in both axial and hoop directions, which opened up an economical pathway for continuous fabrication of biaxially reinforced polyolefin tubes for medical application.