Thermal desorption spectroscopy (TDS) is a powerful method for the measurement of hydrogen concentration in metallic materials. However, hydrogen loss from metallic samples during the preparation of the measurement poses a challenge to the accuracy of the results, especially in materials with high diffusivity of hydrogen, like ferritic and ferritic-martensitic steels. In the present paper, the effect of specimen cooling during the experimental procedure, as a tentative to reduce the loss of hydrogen during air-lock vacuum pumping for one high-strength steel of 1400 MPa, is evaluated. The results show, at room temperature, the presence of a continuous outward hydrogen flux accompanied with the redistribution of hydrogen within the measured steel during its exposure to the air-lock vacuum chamber under continuous pumping. Cooling of the steel samples to 213 K during pumping in the air-lock vacuum chamber before TDS measurement results in an increase in the measured total hydrogen concentration at about 14%. A significant reduction in hydrogen loss and redistribution within the steel sample improves the accuracy of hydrogen concentration measurement and trapping analysis in ferritic and martensitic steels.
No takes yet. Share an insight, caveat, or question.
Fangnon et al. (2020) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: