A significant amount of time and energy is required to dry green timber with a large cross-section. Due to long-lasting internal moisture gradients, internal stress is high during the drying of large cross-sectional timber, and the potential for check occurrence is significant. Although many researchers have aimed to develop a method for drying large pieces of wood without the occurrence of drying defects, a procedure for rapidly drying wood without cracks has not yet been developed. In the present study, an outer surface sealing method and center-boring process (i.e., drilling a hole along the central longitudinal axis) was developed to dry timber with a large cross-section without the occurrence of checks. The proposed center-boring procedure reduces the movement of heat and moisture inside the wood and expedites the drying process by sustaining a small MC gradient. Moreover, the outer surface sealing treatment changes the drying stress direction and controls check occurrence. By kiln drying center-bored (80-mm diameter) and outer-surface-sealed round timber pitch pine (Pinus rigida) with an initial MC of 30% and an outer diameter of 140 mm, a final MC of 6% was obtained within 40 hours without the occurrence of any drying defects.
No takes yet. Share an insight, caveat, or question.
Park et al. (2013) studied this question.
Synapse has enriched 5 related papers. Consider them for comparative context: