A high-capacity phosphonic acid functional adsorbent is prepared by co-condensing oligomers of tetraethoxysilane (TEOS) and trimethoxysilylpropyl diethylphosphonate (DEPPS). Hydrolysis/condensation reactions for both silanes are monitored in the sol-state using 29 Si NMR spectroscopy, and the dependency of the resulting physicochemical properties on these reaction times is investigated. The molar ratio of TEOS to DEPPS is varied to determine the ratio at which high DEPPS incorporation could be attained without evidence of structural perturbation. The phosphonic acid adsorbent is characterized by solid-state 29 Si and 31 P NMR spectroscopy, nitrogen sorption, and elemental analysis. The adsorbent exhibits a ligand density of 10.0 mmol P/g, and maximum values of S BET of 437 m 2 /g, D p of 59 Å, and V p of 0.65 cm 3 /g. Further characterization shows an equilibrium chromium(III) adsorption capacity of 82 mg/g at pH 3.6 and rapid adsorption kinetics. Column adsorption at a high space velocity of 156 h - 1 is achieved with a minimum effluent chromium concentration of 0.01 mg/L. The chromium-loaded adsorbent is stripped using 12 M HCl. A viable synthesis method for the preparation of a high-density functional mesoporous adsorbent is demonstrated.
No takes yet. Share an insight, caveat, or question.
Nam et al. (2005) studied this question.
Synapse has enriched 3 closely related papers on similar clinical questions. Consider them for comparative context: