Dielectric measurements on a single crystal of semicarbazide hydrochloride show three maxima at temperatures of −230, 19, and 21 °C. Initial data for the highest peak clearly suggest a ferroelectric-paraelectric transition with a Curie temperature of 21 °C. In the paraelectric region the Curie law is well followed.