Recently, LiNi 0.8 Co 0.1 Mn 0.1 O 2 has drawn much attention because of its high energy density. Here, 3D-porous LiNi 0.8 Co 0.1 Mn 0.1 O 2 and the one with residual carbon have been synthesized using a resorcinol–formaldehyde-assisted sol–gel approach. Scanning electron microscopy images verify that the synthesized LiNi 0.8 Co 0.1 Mn 0.1 O 2 possesses a 3D-porous morphology. X-ray photoelectron spectroscopy analysis and transmission electron microscopy-mapping images indicate the existence of residual carbon in the secondary particle of 3D-porous LiNi 0.8 Co 0.1 Mn 0.1 O 2 . Furthermore, 3D-porous LiNi 0.8 Co 0.1 Mn 0.1 O 2 with residual carbon exhibits outstanding electrochemical properties. At a current density of 1900 mA g –1, the 3D-porous LiNi 0.8 Co 0.1 Mn 0.1 O 2 with residual carbon can still deliver a reversible capacity of 113 . Moreover, after 150 cycles at 0.2 C, the capacity retention of 3D-porous LiNi 0.8 Co 0.1 Mn 0.1 O 2 with residual carbon reaches to 95%. The excellent electrochemical properties can be ascribed to the unique 3D-porous morphology and residual carbon in the secondary particle.
No takes yet. Share an insight, caveat, or question.
Dong et al. (2018) studied this question.
Synapse has enriched 5 related papers. Consider them for comparative context: