Lithium niobate (LN) microdisk resonators on a LN-silica-LN chip were fabricated using only conventional semiconductor fabrication processes. The quality factor of the LN resonator with a 39.6-μm radius and a 0.5-μm thickness is up to 1.19 × 10(6), which doubles the record of the quality factor 4.84 × 10(5) of LN resonators produced by microfabrication methods allowing batch production. Electro-optic modulation with an effective resonance-frequency tuning rate of 3.0 GHz/V was demonstrated in the fabricated LN microdisk resonator.