ZnO nanoparticles were generated by thermal decomposition of a binuclear zinc (II) curcumin complex as single source precursor. Thermal behavior of the precursor showed a considerable weight loss at about 374 °C by an exothermic reaction with a maximum weight loss rate of 14%/min. Complete decomposition of precursor was observed within 49 min with a heating rate of 10 °C/min. Synthesized nanoparticles have been characterized by X-ray diffraction, Fourier transform infrared spectroscopy, transmission electron microscopy and selected area electron diffraction microscopy. Results revealed monodispersed hexagonal zincite structure with an average size of 117 ± 4 nm.