Experimental study demonstrates wafer-scale pulsed laser deposition of 2D tin selenide with monolayer precision, indicating scalable fabrication for flexible optoelectronics.
Abstract 2D SnSe presents considerable opportunities for transistors, optoelectronics, and photonics if wafer-scale deposition with monolayer thickness control can be achieved. This work answers this critical need by developing a mirror rastering pulsed laser deposition (PLD) approach that enables wafer scale coverage of SnSe with monolayer thickness precision and atomic scale surface roughness (0.29 nm). SnSe thin films are deposited onto 7.5 × 5 cm flexible mica substrate in monolayer increments from 3.5 to 6.1 nm by mirror rastered PLD. All films exhibit stoichiometric (200) oriented Pnma SnSe with consistent phase and thickness across the length of the wafer. Furthermore, sheet resistance is constant with an average of 0.52 GΩ/sq across a 6 cm span and remains stable upon mechanical flexing. This work demonstrates the wafer-scale SnSe deposition with precise thickness control needed to enable next-generation 2D electronics and optoelectronics.
No takes yet. Share an insight, caveat, or question.
Garten et al. (2026) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: