Answers are grounded in this paper and cite their sources.
We present a technique for in situ Raman measurements of suspended individual single-walled carbon nanotubes (SWNTs) under strain. We observe a strong change in the radial breathing mode intensity with increasing strain as the nanotube moves out of (or into) resonance, and for strain greater than approximately 2%, there is a clear irreversible upshift in the G-mode frequencies accompanied by an increase in intensity of a broad peak at a position associated with the D mode. For lower strain, the G-mode peaks (A1, E1, and E2) do not change significantly in position but change in relative intensity.
No takes yet. Share an insight, caveat, or question.
Lee et al. (2007) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: