To determine the effect of BaSO4 on the fatigue crack growth rate, da/dN = C(delta K)n, of poly(methyl methacrylate) (PMMA) bone cement, radiopaque bone cement, radiolucent bone cement, and commercial PMMA (Plexiglas) were tested using a methodology based on ASTM E647. The crack growth rate of radiopaque bone cement was one order of magnitude less than that of radiolucent. Fractographic analysis showed that the regions of rapid catastrophic fracture were smooth for all materials tested. The radiopaque fatigue surface was rough and characterized by ragged-edged stacked plateaus, a morphology consistent with the model of crack propagation through the interbead matrix. Voids were visible in the interbead matrix on the order of the size of BaSO4 particles. The fatigue surface of radiolucent bone cement was relatively smooth, a morphology consistent with crack propagation through both the PMMA beads and interbead matrix. Fatigue striations were visible, and their spacing correlated well with crack propagation rates. The striations indicated an increased crack growth rate through the PMMA beads.
No takes yet. Share an insight, caveat, or question.
Molino et al. (1996) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: