The wake-up effect is a major issue for ferroelectric HfO 2 -based memory devices. Here, two TiN/HZO/TiN structures deposited by magnetron sputtering on silicon are compared. The maximum remanant polarization is higher than 21 μC/cm 2 for both samples, but a strong difference is observed in the electrical behavior. For the mesa sample, the difference between the maximum and initial remanent polarization is only 3 μC/cm 2, whereas it is around 14 μC/cm 2 in the non-mesa case. We discuss the root causes of these behaviors in light of GIXRD results.
No takes yet. Share an insight, caveat, or question.
Bouaziz et al. (2019) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: