Biopersistence of commercial man-made vitreous fibers (MMVF) and crocidolite were studied in Fischer 344 rats. MMVF used were size-selected to be rat-respirable, and rats were exposed nose-only 6 h/day for 5 days to gravimetric concentrations (30 mg/m3) of two fiber glass compositions--a rockwool, and a slagwool--or to 10 mg/m3 of long-fibered crocidolite, or to filtered air. Animals were sacrificed at 1 hr, 1, 5, 31, 90, 180, 270, 365, and 545 days after exposure stopped. Fibers were recovered from digested lung tissue to determine changes in concentrations (fibers/mg dry lung) and fiber retentions (expressed as percent of day 1 retention [PR]) for selected dimension categories. One-day average concentrations of lung-retained MMVF and crocidolite fibers, of diameter > or = 0.5 micron or > 20 microns in length, were nearly equal, permitting direct comparisons between MMVF and crocidolite. At 270 days average PR for MMVF > or = 0.5 micron in diameter were from 3 to 6 +/- 2% and 27 +/- 9% for crocidolite. For fibers > 20 microns, PR were 1 to 4 +/- 4% for MMVF and 37 +/- 20% for crocidolite. At 545 days, MMVF > 20 microns in length were at background level while concentration of crocidolite fibers > 20 microns in length remained at 2000 +/- 400 f/mg DL (dry lung), or 38 +/- 9% of day-1 retention. These results suggest strongly that MMVF dissolved or fractured in vivo whereas crocidolite fibers did not change.
No takes yet. Share an insight, caveat, or question.
Musselman et al. (1994) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: