Vertically aligned titanium dioxide (TiO 2 ) nanotubes were synthesized by electrochemical anodic oxidation in an electrolyte solution containing 0.45 wt% ammonium fluoride (NH 4 F) and 2 vol% deionized water at constant potential (70 V) for various anodization time at the room temperature. The influence of the anodization time on the morphology and optical properties of the anodic TiO 2 nanotubes have been studied. Field emission scanning electron microscopy results revealed that the anodic TiO 2 nanotube morphology extremely depends on the anodization time. It was observed that by increasing anodization time, length of the anodic TiO 2 nanotubes increased and nanotubes destroyed at the top of the tubes. After a long time of anodization process (9 h), nanotubes completely destroyed. Photoluminescence measurements showed that the anodic TiO 2 nanotube band gap energy depends on the anodic TiO 2 nanotube morphology. The anodic TiO 2 nanotubes without any damage had a minimum band gap energy (2.9 eV).
No takes yet. Share an insight, caveat, or question.
Jedi-soltanabadi et al. (2018) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: