We describe the preparation of a chemical vapour deposition (CVD) thin film using the low temperature surface discharge plasma torch of our previous paper, and examine the influences of preparation distance, applied voltage and preparation time on the thin film structure. The composition of the obtained CVD thin film was altered by the applied voltage and preparation distance, and it was made from an inorganic composition with a state of SiO 2 under a high-applied voltage and long preparation distance.